Appearance....................................................................................white
viscous coating, tintable
*Solids by volume ASTM
(D2697)..........................................................................................54%
*Solids by weight ASTM
(D1644)...........................................................................................66%
Toxicity............................................................................................None
(See
MSDS for details)
pH........................................................................................................................................9.0
Density....................................................................................................................11.8
lbs/gal.
Vehicle...............................................................................................................................H2O
*Tensile Strength (initial) ASTM
(D2370)............................................................................245
psi
*Elongation-initial ASTM (D2370O)......................................................................................275%
*After 1000 hours accelerated weathering ASTM
(D2370)......................................................265%
*Permeance
ASTM (D16553A)......................................................................................45
perms
*Water swelling ASTM
(D471)..............................................................................................12%
*Accelerated weathering ASTM
(D4798).....................................................No
cracking or splitting
*Adhesion dry ASTM
C-794...............................................................................9.0
pli (concrete)
*Adhesion wet ASTM C-794...............................................................................3.0
pli (concrete)
*Fungi Resistance (ASTM G21)........................................................zero
rating (no fungal growth)
*Tear
Resistance ASTM
(D624).....................................................................................84
Lbf/in
*Low
temp flexibility ASTM (D522) after 1000 hours
accelerated weathering........................passes
Solar
Reflectance (ASTM E-903).....................................................................91%
UV/IR/Visible
Flame
Resistance ASTM
(E-108)...........................................................Class
A (Factory Mutual)
Simulated hail damage..............................................................................Pass
(Factory Mutual)
Chemical Stain
Resistance....................................Excellent
(1 ist available for specific chemicals)
NOTE:
VALUES/DATA SPECIFIED ARE INCREASED SUBSTANTIALLY
WHEN COMPOUND APPLIED IN CONJUNCTION WITH FLEXIBLE
MAT. ALL INFORMATION HEREIN ACCURATE TO THE BEST OF
OUR KNOWLEDGE
*Denotes test that
comprise the new
ASTM D-6083 standard for liquid applied acrylic
roof coatings. This new standard is the benchmark by
which these types of coatings should be judged.